Table 1 Viscoelastic parameters of NIH/3T3 fibroblast.
From: Local viscoelasticity of living cells measured by rotational magnetic spectroscopy
Wire length | ωC (rad s−1) | η0 (Pa s) |
| G (Pa) |
|---|---|---|---|---|
L=1.9 μm | 0.20±0.05 | 32±8 | 0.8±0.1 | 16±2 |
L=2.8 μm | 0.15±0.02 | 26±5 | 0.8±0.1 | 9±2 |
L=3.0 μm | 0.07±0.02 | 59±15 | 0.8±0.1 | 11±2 |
L=5.9 μm | 0.03±0.01 | 78±20 | 0.6±0.1 | 8±2 |
(rad)
is the angle by which the wire returns back at high frequency and G is the elastic modulus obtained from equation (4). The error bars are defined as s.e.m.