Table 1 Five of the 14 best alloys with the lowest ΔT.

From: Accelerated search for materials with targeted properties by adaptive design

Iterations

Composition

Δ T (K)

Transformation temperature (K)

6

Ti50.0Ni46.8Cu0.9Fe2.0Pd0.3

2.64

289.95

6

Ti50.0Ni44.2Cu1.9Fe3.8Pd0.1

2.53

243.43

6

Ti50.0Ni46.7Cu0.8Fe2.3Pd0.2

1.84

281.77

7

Ti50.0Ni48.1Cu0.2Fe1.5Pd0.2

2.09

301.86

7

Ti50.0Ni46.5Cu1.1Fe2.2Pd0.2

2.32

283.79

  1. DSC, differential scanning calorimetry.
  2. From a total of 9 iterations, which resulted in 36 new alloys, 14 had a ΔT <3.15 K, the lowest in the original training set of 22. Transformation temperature is given by the endothermic peak in the DSC curve.