Figure 4: Investigation of possible mechanisms behind the photocurrent degradation. | Nature Communications

Figure 4: Investigation of possible mechanisms behind the photocurrent degradation.

From: Light-activated photocurrent degradation and self-healing in perovskite solar cells

Figure 4

(a) J–V characteristics before (blue square–pink line) and after 2 h of constant illumination (red triangles–black line); voltages are scanned from forward to reverse (symbols) and from reverse to forward (lines) with delay time of 3 ms (other scan rates are presented in Supplementary Information and do not show hysteresis). (b) VOC evolution over several light on (red curves) and light off (space in between) cycles. (c) Control measurement of time evolution of the photocurrent by applying a forward bias when the device is rested in the dark (red circles) in comparison to the constantly illuminated device (black line).