Figure 6: Particle fracturing in chemically delithaiated LixMn1.5Ni0.5O4 crystals. | Nature Communications

Figure 6: Particle fracturing in chemically delithaiated LixMn1.5Ni0.5O4 crystals.

From: Phase transformation mechanism in lithium manganese nickel oxide revealed by single-crystal hard X-ray microscopy

Figure 6

(a) 3D surface renderings of two selected Mn1.5Ni0.5O4 crystals (the left one at 4 μm and the right one at 2 μm) show the formation of irregularly shaped cracks on the particle surface, (b,c) SEM images of pristine LiMn1.5Ni0.5O4 and delithiated Mn1.5Ni0.5O4 crystals, respectively. Scale bars, 1 μm (ac).

Back to article page