Figure 7: Young’s modulus and elongation ratio at break of NSG hydrogels. | Nature Communications

Figure 7: Young’s modulus and elongation ratio at break of NSG hydrogels.

From: Nano-structured smart hydrogels with rapid response and high elasticity

Figure 7

(a,b) Effects of ANG polymerization time (a, NIPAM concentration is fixed as 1.5 mol l−1) and NIPAM monomer concentration (b, tp=40 min) on the Young’s moduli (E) of NSG hydrogels at the tensile strain of 50%. (c,d), Effects of ANG polymerization time, NIPAM monomer concentration and ANG nanogel concentration on the elongation ratio at break (εb) of NSG hydrogels of various compositions at room temperature (c) and body temperature (d).