Table 2 The wood species from Nanhai No. 1 shipwreck and the corrosion degrees

From: Microbial erosion assessment on waterlogged archaeological woods (WAWs) from a Chinese ancient shipwreck, Nanhai No. 1

Sample no.

Excavate quadrat-wood number

Wood species

Corrosion degreea

1

2014NHI-T0301-W9

Pinus massoniana

Absent

2

2014NHI-T0601-W19

Pinus massoniana

Weak

3

2014NHI-T0502-W9

Pinus massoniana

Weak

4

2014NHI-T0102-W7

Alnus trabeculosa

Weak

5

2014NHI-T0301-W13

Pinus massoniana

Weak

6

2014NHI-T0502-W7

Mussaendopsis beccariana

Moderate

7

2014NHI-T0502-W24

Pinus massoniana

Weak

8

2014NHI-T0502-W17

Fokienia hodginsii

Absent

9

2014NHI-T0102-W5

Pinus massoniana

Moderate

10

2014NHI-T0201-wide portside

Alnus trabeculosa

Severe

11

2014NHI-T0301-W12

Terminalia hainanensis

Total

12

2014NHI-T0301-W4

Terminalia hainanensis

Severe

13

2014NHI-T0602-W1

Alnus trabeculosa

Severe

14

2014NHI-T0102-W12

Pinus massoniana

Absent

15

2014NHI-T0502-W2

Mischocarpus oppositifolius

Absent

16

2014NHI-T0501-W3

Pinus massoniana

Moderate

17

2014NHI-T0302-W1

Terminalia hainanensis

Severe

18

2014NHI-T0301-W6

Terminalia hainanensis

Total

19

2014NHI-T0301-W13

Mussaendopsis beccariana

Total

20

2014NHI-T0201-W1

Fokienia hodginsii

Absent

  1. aAccording to Klaassen [32]