Table 2 Quantitative results of XRF analysis of three stone samples (wt %)

From: The deterioration process of limestone in the Anahita Temple of Kangavar (West Iran)

Sample

CaO

SiO2

MgO

Al2O3

Fe2O3

CuO

K2O

ZnO

SO3

SrO

TiO2

MnO

PbO

Cl

Na2O

Rb2O

LOIa

K3

49.74

8.13

2.53

0.42

0.40

0.22

0.09

0.08

0.04

0.03

0.03

0.02

38.18

K4

31.97

2.83

17.66

0.30

2.03

0.31

0.06

0.13

0.02

0.01

0.11

0.02

0.02

44.37

K11

38.54

11.60

5.81

4.71

2.24

0.09

1.16

0.03

0.06

0.02

0.24

0.03

0.20

0.60

35.12

  1. aLoss on ignition (1000 °C, 2 h)