Fig. 11: SEM BSE images.
From: Beyond the aesthetics of Tang and Liao dynasties artifacts in the British Museum’s collection

a Beaded rim decoration on the 6-lobed bowl (2022,3034.22). b Areas of SEM-EDX analysis showing gradual increase in nitrogen (N) and sulphur (S) from the beads towards the join (from spectrum 5 to spectrum 8). c Heat damage on some beads at the join, appearing slightly melted, likely due to excessive heat during soldering.