Fig. 2: EELS elemental maps and corresponding HAADF TEM images of the as-cast Fe-containing glass
From: On cryothermal cycling as a method for inducing structural changes in metallic glasses

(a) and after 10 cryothermal cycles (b) and the Ni-containing glass after 10 cryothermal cycles (c)