Fig. 5
From: In situ wrapping of the cathode material in lithium-sulfur batteries

Suppression of polysulfide shuttling using in situ wrapping. a Shuttle current profiles of CMK-3/S, CMK-3/S@PANS, and CMK-3/S@PANS@TPS cathodes and a CMK-3/S cathode in an electrolyte with 1 wt% lithium nitrate (measured at a constant holding potential of 2.28 V). b UV–vis absorption spectra of the electrolytes after 20 cycles with various cathodes in glass cells at 0.1 C. c–e Photographs of CMK-3/S, CMK-3/S@PANS, and CMK-3/S@PANS@TPS cathodes after 20 cycles at 0.1 C in sealed glass cells