Fig. 5

In situ XRD analysis of the interactions during cycling. a XRD intensity heat map from 4 to 8.5o of a 2.4 mg cm–2 cell’s first cycle discharge at 54 mA g–1 and charge at 187.5 mA g–1, where triangles = Li2S, square = AQ, asterisk = sulfur, and circle = potentially polysulfides 2θ. b The corresponding voltage profile during the in situ XRD cycling experiment