From: Crystallographic character of grain boundaries resistant to hydrogen-assisted fracture in Ni-base alloy 725

Fig. 1

3D sample reconstruction. a X-ray attenuation tomography (XRAT) data with metal shown in gray and void space inside the secondary crack shown in black. Scale bar: 200 μm. b Isolated section of the XRAT reconstruction with an edge-on view of the nominal crack plane (XY), indicated in blue. The nominal crack propagation direction (X) is into the page. c High-energy diffraction microscopy (HEDM) reconstruction of the microstructure viewed from the same direction as b. Each voxel is colored according to the crystallographic orientation of the crystal at that location relative to the laboratory reference frame. Scale bar for b and c: 100 μm. The black void space indicating the space inside the crack was obtained from the XRAT reconstruction and digitally fused with the HEDM data