Fig. 1: The DSC curve of the as-prepared Ce65Al10Co25 MG from 330 K to 625 K with a heating rate of 10 K per minute.
From: Two-way tuning of structural order in metallic glasses

The sample undergoes relaxation below the glass transition temperature, Tg ~ 410 K. The first exothermic peak starts at T1 ~ 428 K and is followed by three complex reactions starting at T2 ~ 483 K.