Fig. 2: Flux patterns measured at different tensile strains.
From: Probing of the internal damage morphology in multilayered high-temperature superconducting wires

The exerted strains under zero-field-cooled conditions at 64 mT and 40 K from (a) to (f) are 0%, 0.40%, 0.72%, 0.75%, 0.78%, and 0.80%, respectively. Here, the scale bar represents 500 μm.