Fig. 6: The structural evolution of lithiated graphite with the electrolyte during heating. | Nature Communications

Fig. 6: The structural evolution of lithiated graphite with the electrolyte during heating.

From: In situ observation of thermal-driven degradation and safety concerns of lithiated graphite anode

Fig. 6

a The HEXRD plots of LiC6 (001) Bragg reflection evolution from 25 to 66 °C. b The HEXRD plots of lithiated graphite anode with electrolyte from 25 to ~280 °C with 2 °C/min. The 2θ value has been converted into d-spacing following Bragg’s rule. c The comparison of the phase evolution of the lithiated graphite anode with and without the presence of electrolyte. The lithium melting point (MP) 180 °C is also described in the figure.