Fig. 5: Comparison of \(\left[2\bar{1}\bar{1}0\right]\) diffraction patterns for select alloys and processing conditions. | Nature Communications

Fig. 5: Comparison of \(\left[2\bar{1}\bar{1}0\right]\) diffraction patterns for select alloys and processing conditions.

From: Elimination of oxygen sensitivity in α-titanium by substitutional alloying with Al

Fig. 5

a \(\left[2\bar{1}\bar{1}0\right]\) diffraction pattern of a water-quenched Ti-6Al-0.3 O alloy. b \(\left[2\bar{1}\bar{1}0\right]\) diffraction pattern of an aged Ti-6Al-0.3 O alloy. The white arrows indicate the diffuse scattering of the Ti3Al superlattice. c \(\left[2\bar{1}\bar{1}0\right]\) diffraction pattern of an aged Ti-6Al alloy. The dashed white arrows indicate a very weak diffuse scattering of the Ti3Al superlattice. The corresponding normalized intensity profiles along dotted lines in each figure are shown below.

Back to article page