Fig. 3: Structure characterization of the 15CuCe catalyst after 240 h stability test.

a TEM image; b‒d STEM images and element mapping results. e‒h HAADF-STEM images; i Enlarged image of the highlighted region in (h); j Scheme of structural evolution for the copper‒ceria catalyst during long-term stability test.