Fig. 5: Coordination number distribution in Gd2Zr2O7 and Ca1.2Gd0.8Zr0.8Nb0.6Ta0.6O7 (HEPO) during crack propagation along with the experimental observations.
From: Ultra-dense dislocations stabilized in high entropy oxide ceramics

a, b The surface crack propagation path in Gd2Zr2O7 and HEPO samples; c Straight and brittle crack propagation in Gd2Zr2O7 crystal; d Crack bridging in HEPO interacting with two edge dislocations; e Crack deflection in HEPO interacting with two edge dislocations. Dislocations are indicated by red arrows. The color scale denotes the coordination number of each cation (unit: counts).