Fig. 6: Measurements of depression morphology during laser line scanning for experiments without and with powder.
From: The interplay between vapour, liquid, and solid phases in laser powder bed fusion

a Depression depth variation with input energy density. b Calculated drill rate based on experimental depth. c Measured and predicted front wall angle, according to tanθ = D/d. All three graphs use the same legend shown in (c).