Table 1 Tight-binding parameters. These parameters (in units of meV) were used for Eqs. (4), (5), (6), and (7), yielding Fig. 5a
From: The superconductivity of Sr2RuO4 under c-axis uniaxial stress
∣εzz∣ | μ1D | t1 | t2 | t3 | t4 | t5 | t6 | t7 | μ2D | \({\bar{t}}_{1}\) | \({\bar{t}}_{2}\) | \({\bar{t}}_{3}\) | \({\bar{t}}_{4}\) | \({\bar{t}}_{5}\) | \({\bar{t}}_{6}\) | \({\bar{t}}_{7}\) | \({\bar{t}}_{8}\) | \(\tilde{t}\) | η1 | η2 |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
0.00 | 316 | 296 | 53 | − 16 | 17 | − 57 | − 15 | − 12 | 433 | 370 | − 6 | 123 | 20 | 14 | 3 | 3 | − 2 | 9 | − 51 | − 51 |
0.0075 | 294 | 284 | 54 | − 16 | 18 | − 56 | − 15 | − 10 | 437 | 369 | − 5 | 122 | 20 | 14 | 3 | 3 | − 3 | 10 | − 51 | − 51 |
0.015 | 273 | 271 | 55 | − 17 | 19 | − 55 | − 15 | − 9 | 441 | 368 | − 5 | 121 | 20 | 13 | 3 | 3 | − 3 | 10 | − 51 | − 51 |
0.020 | 259 | 264 | 56 | − 18 | 20 | − 55 | − 15 | − 8 | 443 | 367 | − 4 | 120 | 20 | 13 | 3 | 3 | − 3 | 11 | − 52 | − 51 |