Fig. 3: Electrochemical performance and structure evolution of NVO cathode in WSE. | Nature Communications

Fig. 3: Electrochemical performance and structure evolution of NVO cathode in WSE.

From: A weakly solvating electrolyte towards practical rechargeable aqueous zinc-ion batteries

Fig. 3

a GCD curves at 0.1 A g−1, b rate capability comparison and c cycling stability comparison at 5 A g−1 of Zn/NVO cells in LCE and WSE. The inset in Fig. 3c is the enlarged cycling stability at 5 A g−1 of Zn/NVO cells in LCE and WSE. d GCD curves of NVO electrode using WSE at 0.1 A g−1, e ex-situ XRD patterns and f corresponding contour map. g TG curves and h XRD patterns of NVO electrode after 50 cycles at 0.1 A g−1 in LCE and WSE. i Diffusivity coefficient at various states of discharge in LCE and WSE according to GITT measurement.