Fig. 3: In situ Raman results of [Li(G4)][FSI] on single-layer graphene surface.

From: Unraveling the energy storage mechanism in graphene-based nonaqueous electrochemical capacitors by gap-enhanced Raman spectroscopy

Fig. 3

a In-situ Raman spectra of [Li(G4)][FSI] at Au@SiO2/single-layer graphene/Au. The purple Raman spectra correspond to the potential being negative relative to PZC, while the blue Raman spectra correspond to the potential being positive relative to PZC. b Proposed adsorption configuration of [Li(G4)][FSI] at single-layer graphene in different potential region (including E < PZC, E = PZC and E > PZC). F, S, O, N, C, H, and Li atoms are shown in green, yellow, red, cyan, gray, blue, and reseda, respectively.