Fig. 2: Characterization of nanostructure and composition of SEI. | Nature Communications

Fig. 2: Characterization of nanostructure and composition of SEI.

From: Robust bilayer solid electrolyte interphase for Zn electrode with high utilization and efficiency

Fig. 2

a HRTEM images of Zn surface with no SEI formation in ZnSO4 electrolyte. b, c HRTEM images of bilayer SEI on the Zn surface in ZnSO4-DMI electrolyte. d STEM image of bilayer SEI on the Zn surface. ei The corresponding EDS mapping of (d). jl Fast Fourier transform on three representative regions of the SEI outer layer. m-u, Actual vs. theoretical reciprocal space of (mo) ZnO-mp-2133, (pr) ZnCO3-mp-9812 and (su) Zn(CO2)2-mp-559437 in different crystal regions.