Fig. 7: Electrochemical performance of Zn full cells with low N/P ratios and high ZURs (25 °C).
From: Robust bilayer solid electrolyte interphase for Zn electrode with high utilization and efficiency

a Long-term stability of Zn | |AC full cells with/without the bilayer SEI at N/P of 2. b GCD curves of Zn | |AC full cell with the bilayer SEI at N/P of 2. c Long-term stability of Zn | |I2 full cells with/without the bilayer SEI at N/P of 1.5. d GCD curves of different cycles of Zn | |I2 full cell with the bilayer SEI at N/P of 1.5. e GCD curve of anode-free Zn | |Br pouch cell with the bilayer SEI (The discharge current is 40 mA). f Long-term stability of anode-free Zn | |Br pouch cell with the bilayer SEI (The discharge current is 40 mA). g An LED digital screen powered by anode-free Zn | |Br pouch cell with the bilayer SEI.