Table 1 Magnetic properties of canted GdxCo100−x moments with different magnetic canting angles in this study
Magnetic Property | Sample-45 | Sample-56 | Sample-13 |
---|---|---|---|
As Deposited Atomic Concentration | Gd24.7Co75.3 | Gd24.7Co75.3 | Gd24Co76 |
Relative Degree of Oxidation Treatment | Intermediate | Light | Heavy |
Canting Angle of Easy Axis (∘) | 45 | 56.25 | 13.5 |
Saturation Magnetization Ms (emu/cc) | 40 | 94 | 111 |
IP Remanent Magnetization Mr,ip (emu/cc) | 37 | 44 | 17 |
OOP Remanent Magnetization Mr,oop (emu/cc) | 20 | 75 | 102 |
IP Coercive Field Bc,ip (G) | 180 | 87 | 49 |