Fig. 4: Durability of the SiP/F-MOFs@ATP coating. | Nature Communications

Fig. 4: Durability of the SiP/F-MOFs@ATP coating.

From: Scalable robust photothermal superhydrophobic coatings for efficient anti-icing and de-icing in simulated/real environments

Fig. 4

Changes in CA and SA of the coating during the (a) Taber abrasion test, (b) tape-peeling test, and (c) UV aging test. df SEM images of the coating after 150 cycles Taber abrasion. Data in (a, b) are shown as mean ± SD, n = 5. Data in (c) are shown as mean ± SD, n = 3. Source data are provided as a Source Data file.