Fig. 4: Structure and oxygen evolution.
From: Multicationic interactions mitigating lattice strain in sodium layered cathodes

Contour plots of in situ XRD patterns and the corresponding crystal parameters evolution of (a, c) NFM, and (b, d) CFTS5 cathodes. Charge compensation mechanism in CFTS5 cathodes. Ex-situ XANES spectra and the corresponding EXAFS spectra at the (e, f) Mn, (g, i) Ni, and (h, j) Fe K-edges of CFTS5 at different charge/discharge states. DEMS data during the initial cycle of (k) NFM and (l) CFTS5 cathodes (active mass loading of ~10 mg cm−2).