Fig. 1: Electrodeposition of a lithium layer.
From: Purity of lithium metal electrode and its impact on lithium stripping in solid-state batteries

Voltage profile during lithium electrodeposition at the steel|LPSCl interface using a current density of 50 µA cm−2 and schematic of the used cell setup steel|LPSCl|LiLP|steel before and after the lithium deposition. Herein LiLP is a lithium foil with low purity and LiD the electrodeposited lithium.