Fig. 7: The target displacement following the y-direction inputted for the first case study.
From: Computational design for 4D printing of topology optimized multi-material active composites

The beam—fixed on the left side—exhibits a large deflection (76 mm) once thermally stimulated (from 40 °C to 80 °C).