Table 1 Statistical data on grains in upper half part of μg and 1g samples
From: Role of hydrostatic pressure and wall effect in solidification of TC8 alloy
Sample | Grain number per unit area (mm−2) | Grain size (μm) | Aspect ratio | ||||
---|---|---|---|---|---|---|---|
Ave. | Max. | Min. | Ave. | Max. | Min. | ||
μg | 3.126 | 595 | 1512 | 187 | 2.385 | 6.177 | 1.054 |
1g | 3.807 | 543 | 1202 | 167 | 2.966 | 7.345 | 1.058 |