Pyrolyzation temperature (°C) | \({{R}} = \frac{{{{I}}_{{{\mathrm D}}}}}{{{{I}}_{{{\mathrm G}}}}}\) | La (nm) |
---|---|---|
500 | 4.76 | 1.04 |
600 | 2.90 | 1.71 |
700 | 2.36 | 2.10 |
800 | 2.07 | 2.39 |
950 | 1.33 | 3.73 |