Table 1 Quantitative STEM-EDS point analysis results (average ± 3σ) for matrix and carbides in quenched Cu-added alloy (mass%)
From: Corrosion-resistant carbide-reinforced martensitic steel by Cu modification
Fe | Cr | W | Cu | C | |
|---|---|---|---|---|---|
Matrix | 82.87 ± 7.68 | 12.36 ± 1.32 | 1.89 ± 0.78 | 2.88 ± 0.49 | – |
Primary carbide | 34.20 ± 3.54 | 51.75 ± 5.09 | 8.28 ± 2.95 | 0.48 ± 0.29 | 5.29 ± 1.07 |
Secondary carbide | 37.14 ± 3.67 | 45.03 ± 4.36 | 11.44 ± 3.77 | 1.63 ± 0.42 | 4.76 ± 0.86 |