Fig. 6: SR-IR spectra for the corroded ISG samples. | npj Materials Degradation

Fig. 6: SR-IR spectra for the corroded ISG samples.

From: Near-field corrosion interactions between glass and corrosion resistant alloys

Fig. 6

a ISG(+SSNaCl), b ISG(+PTFENaCl), c ISG(+SSDIW), d ISG(+PTFEDIW). For each sample, the spectra were collected from two different locations, including the area in direct contact with SS or PTFE (contact side) and the area in contact with PFA container (Back side). Spectrum acquired from pristine ISG was also plotted for as a reference.