Table 1 List of experimental groups and testing conditions for SS and glass corrosion.
From: Near-field corrosion interactions between glass and corrosion resistant alloys
Sample ID | Materials | Solution | Temperature | Duration |
---|---|---|---|---|
SLSG-SS-NaCl | SLSG + SS 316 | 0.6 M NaCl | 90 °C | 14 Days |
SLSG-PTFE-NaCl | SLSG + PTFE | 0.6 M NaCl | 90 °C | 14 Days |
SLSG-SS-DIW | SLSG + SS 316 | DI water | 90 °C | 14 Days |
SLSG-PTFE- DIW | SLSG + PTFE | DI water | 90 °C | 14 Days |
SLSG-G30-NaCl | SLSG + Alloy G30 | 0.6 M NaCl | 90 °C | 14 Days |
SLSG-A625-NaCl | SLSG + A625 | 0.6 M NaCl | 90 °C | 14 Days |
ISG-SS-NaCl | ISG + SS 316 | 0.6 M NaCl | 90 °C | 30 Days |
SS-PTFE-NaCl | SS 316 + PTFE | 0.6 M NaCl | 90 °C | 30 Days |
ISG-PTFE-NaCl | ISG + PTFE | 0.6 M NaCl | 90 °C | 30 Days |
ISG-SS-DIW | ISG + SS 316 | DI water | 90 °C | 30 Days |
SS-PTFE-DIW | SS 316 + PTFE | DI water | 90 °C | 30 Days |
ISG-PTFE-DIW | ISG + PTFE | DI water | 90 °C | 30 Days |