Fig. 2: SEM/EDS analysis for SS corroded in close proximity to I-APT.
From: Corrosion interactions between stainless steel and lead vanado-iodoapatite nuclear waste form part I

a A typical area within the center of the crevice. b A typical area outside crevice. c An area near the crevice mouth where massive precipitation was observed. The red box shows where the EDS elemental mapping was acquired. d EDS elemental mappings of precipitates observed near the crevice mouth.