Fig. 1: Stainless-steel and iodoapatite corrosion interaction. | npj Materials Degradation

Fig. 1: Stainless-steel and iodoapatite corrosion interaction.

From: Corrosion interactions between stainless steel and lead vanado-iodoapatite nuclear waste form part II

Fig. 1

Schematic illustration of the experimental setup for SS and I-APT corrosion and the surface morphologies of two groups of I-APT samples, one rectangular and one round shape, corroded in close proximity to SS in 0.6 M NaCl solution for 28 days. The image of the rectangular sample was taken by SEM and the image of the round sample by OM.

Back to article page