Fig. 5: Cross-sectional SEM images and corresponding EDS line scan of the outer surface of Cr-coated Zr tube oxidized at different conditions.
From: Oxidation behavior of Cr-coated zirconium alloy cladding in high-temperature steam above 1200 °C

a, b 1200 oC/0.5 h, c, d 1200 oC/1 h, e, f 1200 oC/2 h, g, h 1200 oC/4 h, i, j 1300 oC/0.5 h, k, l 1300 oC/1 h.