Fig. 7: Microstructures and compositions at the interface of layers 6/7 in Fig. 4.
From: Oxidation behavior of Cr-coated zirconium alloy cladding in high-temperature steam above 1200 °C

a HAADF and d TEM images of ZrO2, ZrCrFeO, and Zr(Cr,Fe)2, and corresponding b EDS mappings and c EDS line scan; SEAD patterns of e ZrO2, f ZrCrFeO, and g Zr(Cr,Fe)2.