Fig. 8: Microstructures and compositions at the interface of layers 7/8 in Fig. 4.
From: Oxidation behavior of Cr-coated zirconium alloy cladding in high-temperature steam above 1200 °C

a HAADF and d TEM image of Zr(Cr,Fe)2, Cr and ZrO2, and corresponding b EDS mappings and c EDS line scan; SEAD patterns of e Cr and f ZrO2.