Fig. 11: A schematic illustration of the crevice corrosion experiment setup used in this study. | npj Materials Degradation

Fig. 11: A schematic illustration of the crevice corrosion experiment setup used in this study.

From: Long-term interactive corrosion between International Simple Glass and stainless steel

Fig. 11

a A SS coupon is sandwiched between two ISG coupons. PTFE plates are placed on the ISG coupons and intimate contact is established with PTFE nuts and bolts. This assembly of samples is then placed in PFA jars. b An illustration of the jar used for 0.6 M NaCl solution. c An illustration of the jar used for silica saturated 0.6 M NaCl.