Fig. 3: Morphology of secondary phase precipitation on SS(+ISG). | npj Materials Degradation

Fig. 3: Morphology of secondary phase precipitation on SS(+ISG).

From: Long-term interactive corrosion between International Simple Glass and stainless steel

Fig. 3

a Secondary phase precipitation on SS(+ISG) for 0.6 M NaCl outside the crevice mouth. b Chemical composition of precipitates determined at points 1 and 2 in (a). c Secondary phase precipitation on SS(+ISG) for silica-saturated NaCl outside the crevice mouth. d Chemical composition of precipitates determined at 2 regions (1 and 2 in inset c’) by EDS.