Fig. 4: Optical Profilometry of ISG.
From: Long-term interactive corrosion between International Simple Glass and stainless steel

a Localized attack on ISG(+SS) corroded in 0.6 M NaCl. b Optical Profilometry of pristine ISG.
From: Long-term interactive corrosion between International Simple Glass and stainless steel
a Localized attack on ISG(+SS) corroded in 0.6 M NaCl. b Optical Profilometry of pristine ISG.