Fig. 12: Multiple characterization results of CaS·xMgO·yAl2O3·TiN inclusions. | npj Materials Degradation

Fig. 12: Multiple characterization results of CaS·xMgO·yAl2O3·TiN inclusions.

From: A critical review of the recent advances in inclusion-triggered localized corrosion in steel

Fig. 12

a, h Morphology of typical target CaS·xMgO·yAl2O3·TiN inclusions and the corresponding element distribution. b Topography map, c potential map and d conductive map of the same region shown in a. eg The strip profile analysis results of the target inclusions shown in a. i The KAM map of the same region shown in h22.