Fig. 8: Independent verification of two feasible models for Al alloys field exposure data. | npj Materials Degradation

Fig. 8: Independent verification of two feasible models for Al alloys field exposure data.

From: Random forest incorporating ab-initio calculations for corrosion rate prediction with small sample Al alloys data

Fig. 8

a Comparison of RF models trained by the pure experimental corrosion dataset or ab-initio calculation modified dataset. b Three different Al alloys, AA5083, AA6N01, and AA7N01, were placed in Southeast Asia (Singapore, Jakarta, and Bangkok) for 2 years to examine the generalization ability of the RF model with phase calculation. c Corrosion morphology and statistics on the number and depth of pits in Al alloys after field exposure.