Fig. 5: EPMA results of the elemental distribution near the white etching zone of the loaded Hastelloy N after 240 h in molten salt.
From: Stress-assisted corrosion behaviour of Hastelloy N in FLiNaK molten salt environment

a C, b Cr, c Ni, and d Mo.