Fig. 12: The characteristics and in-situ corrosion behavior of CaS/CaO–MgO–Al2O3 Cu-containing inclusion.
From: Role of segregation behavior of Cu and Sb in the region of inclusions on initial corrosion

a SKPFM analysis of the CaS/CaO–MgO–Al2O3 inclusion. b EDS analysis of the CaS/CaO–MgO–Al2O3 inclusion. c Corrosion morphology of the CaS/CaO–MgO–Al2O3 inclusion after different times of immersion.