Fig. 10: Cross-SEM and EDS of the surface of Mg-4Li-1Ca alloy after different immersion times containing BSA at different concentrations of Glu. | npj Materials Degradation

Fig. 10: Cross-SEM and EDS of the surface of Mg-4Li-1Ca alloy after different immersion times containing BSA at different concentrations of Glu.

From: Exfoliation of an extruded Mg-4Li-1Ca alloy in presence of glucose and bovine serum albumin

Fig. 10

a 1 g·L−1 Glu + BSA 90 D, b 1 g·L−1 Glu + BSA 120 D, c 1 g·L−1 Glu + BSA 150 D, d 1 g·L−1 Glu + BSA 180 D, e 2 g·L−1 Glu + BSA 90 D, f 2 g·L−1 Glu + BSA 120 D, g 2 g·L−1 Glu + BSA 150 D, h 2 g·L−1 Glu + BSA 180 D, i 3 g·L−1 Glu + BSA 90 D, j 3 g·L−1 Glu + BSA 120 D, k 3 g·L−1 Glu + BSA 150 D, l 3 g·L−1 Glu + BSA 180 D.

Back to article page