Fig. 12: SEM images of QHXC-3 glaze cross-section.
From: The corrosion mechanism of lead-glazed pottery in Han dynasty

a, b Hemispherical adherent deposit of glaze. c Surface morphology of the hemispherical adherent deposit. d, e Surface topography of the inner subsurface of the hemispherical adherent deposit.