Fig. 3: Surface morphologies of AM porous Zn alloy after immersion test.

Degradation profile of (a) D, (b) F, (c) G, and (d) P scaffolds after removal of the degradation products by different immersion time points. (arrows: local degradation).
Degradation profile of (a) D, (b) F, (c) G, and (d) P scaffolds after removal of the degradation products by different immersion time points. (arrows: local degradation).