Fig. 1: Characterization of as-deposited Ta coating on short smooth tube.
From: Failure mechanism of sputtered Ta coatings on short rifled gun bore under vented vessel tests

a cross-sectional morphology by SEM; b XRD patterns; c cross-sectional morphology by TEM; d Enlarged morphology in the large red circles, and the corresponding NBDs in the small red circles.